| Place of Origin: | China |
| Brand Name: | BaiZhuang |
| Certification: | UL File No.: QMFZ2.E352175 |
| Model Number: | BZ-6800(WT) |
| Document: | 6800A_B _ UL Product iQ.pdf |
This is a high-performance white potting compound - BZ-6800(WT) polyurethane potting compound, which is a UL94-V0 certified polyurethane material (UL certification No.: QMFZ2.E352175). It not only complies with RoHS and REACH standards but also features excellent structural strength, superior adhesion to substrates, outstanding mechanical properties, and superior electrical performance. Therefore, it is widely used as a potting material in electronic products and electrical equipment.
1. Low viscosity, compatible with both manual operation and automated equipment applications
2. Exceptional resistance to extreme low and high temperature conditions
3. Superior electrical insulation performance and reliable operational stability
4. Top-tier flame retardant capabilities, holding a UL94-V0 fire safety rating
5. Outstanding waterproof and moisture-proof characteristics, boasting an ultra-low water absorption rate
6. Strong adhesive properties for bonding with commonly used plastics and metal materials
|
Parameters |
Hardener BZ-6800(WT) A |
Resin BZ-6800(WT) B |
|
|
Before curing |
Appearance |
Brown liquid |
Wihte liquid |
|
Viscosity(mPa·s.25℃) |
150±100 |
3700±1300 |
|
|
Initial mixed viscosity(mPa·s.25℃) |
1300±300 |
||
|
Density(g/cm³.25℃) |
1.15±0.05 |
1.53±0.05 |
|
|
Mixing&Curing
|
Mix ratio(by weight) |
A:B=20:100 |
|
|
Pot life 130±30g(min.25℃) |
25±10 |
||
|
Curing condition |
Room temperature curing |
||
|
Surface drying time 30g(H.25℃) |
6-9 |
||
|
Curing time 30g(H.25℃) |
9-13 |
||
|
Curing time(Heated) |
60℃ heated 1-2H |
||
|
After curing
|
Color |
White |
|
|
Hardness (Shore A) |
40-55 |
||
|
Temperature resistance(℃) |
-40~120℃ |
||
|
Flame retardancy UL94 (vertical burning) |
V-0(3mm) |
||
|
Water absorption(24H) |
≤0.5% |
||
|
Thermal conductivity(W/m.k) |
≥0.5 |
||
|
Surface resistivity(Ω/sq) |
≥1.0×1013 |
||
|
Volume resistivity(Ω.cm) |
≥1.0×1013 |
||
|
Tensile strength(MPa) |
≥3 |
||
|
Elongation at break(%) |
≥50% |
||
|
Dielectric constant(at 50Hz) |
≥6 |
||
|
Breakdown voltage(kV/mm) |
≥18 |
||